Metallurgical Principles and Practice of Engineering (PE) Study Guide: Question #26


It Is the Policy of The Minerals, Metals & Materials Society (TMS) to Encourage the Professional Registration of Metallurgical Engineers.

Choose the appropriate thermal and/or mechanical treatment for Alloy C-276 (UNS N60276, formerly known as Hastelloy C-276) for subsequent machining, then use in a corrosion resistant application.

(A)
Cold work 15%
(B)
Cold work 15%, heat at 1,200°F (650°C) for 1 hours, air cool
(C)
Heat at 2,050°F (1,120°C) for 30 minutes, quench
(D)
Heat at 2,050°F (1,120°C) for 30 minutes, quench, heat at 1,200°F (650°C) for 1 hour, air cool