Figure 5. The effect of alloying and coating type on the wettability kinetics in the Al/Al2O3 system: showing (a-top) a comparison between aluminum and Al-Si droplets on alumina substrates coated with Cr-42Si-9W at 1,023 K and (b-bottom) Al-10Ti alloy on metallized alumina substrate at 1,123 K.252
 